Swaging .224 Overview (Part 1)
Several people wanted a video after my bullets were featured on Elvis Ammo's channel, so this is what I was able to cover of the swaging process without having my point form die that's out for repair, or any 22lr brass on hand. I'll complete this once I have them in hand. Even so, I hope it's more informative than the swaging videos I found when looking into swaging for myself.
Admittedly, it is a time consuming process, but the results are cheap jacketed .224 bullets that can be pushed over 3000 fps.
I ultimately decided to go the swaging route for .223 because COWW aren't readily available in my area and Rotometals can get expensive. Not having to harden my alloy keeps costs low.
I had to redo some parts, so I hope I didn't cover things multiple times.
►I'm using a BT Sniper Deluxe kit for swaging .224 flat base and rebated boat tail bullets (a one-off custom order RBT kit).
http://castboolits.gunloads.com/forumdisplay.php?114-BT-Sniper
I see that I forgot to show the base punch with the rubber on it, that one's used when point forming RBTs.
Disclaimer: I am not affiliated with BT Sniper.
►He're a list of the steps involved. It's involved, but not nearly as overwhelming as it seems since some steps can be done in bulk and set aside (if this old geezer can do it, you can too):
BRASS:
1) Wet tumble brass (1 Tablespoon Dawn, 1/4 tsp Lemishine)
2) Derim brass
3) Wet tumble brass (1 Tablespoon -Dawn- Woolite, 1/4 tsp Lemishine)
4) Anneal brass
5) Wet tumble brass (1 Tablespoon Dawn, 1/2 tsp Lemishine)
6) Sort brass by headstamp
7) Sort brass by weight
LEAD:
1) Cast cores
2) Size cores
3) Remove excess lead "foil" from cores
4) Wash cores
5) Sort cores by weight
STEP THE NEXT:
1) Insert cores into brass (core shaker)
2) Seat cores
3) Remove excess lube by rolling on towel
3) Form point
4) Wet tumble (15 min)
5) Inspect
LOAD THEM IN CARTRIDGES AND HEAD TO THE RANGE!!!
►Here's a bit more info you might be interested in:
Corbin Handbook of Bullet Swaging No. 9:
http://www.swage.com/ebooks/hb9-text.pdf
Scroll down to "About Weight Control..."
http://www.corbins.com/csw.htm
Some info about Rebated Boat Tails:
http://www.swage.com/ftp/rbt.pdf
Category | None |
Sensitivity | Normal - Content that is suitable for ages 16 and over |
Related Videos
Range Report- Heavies Made With New Trimmer Setup
7 months, 1 week ago
7 months, 3 weeks ago
7 months, 4 weeks ago
11 months, 1 week ago
11 months, 3 weeks ago
Russian Slug Mold Core Pin Protectors
1 year ago
Warning - This video exceeds your sensitivity preference!
To dismiss this warning and continue to watch the video please click on the button below.
Note - Autoplay has been disabled for this video.